Add to Cart
Refractory anchor brick to fire brick containing Al2O3 more than 48%, which is made of high grade bauxite through high temperature calcinations. Fire clay brick is a kind of neutral refractory material so that it enjoys excellent resistance to acid and alkali corrosion.
Feature:
Fire clay brick has the feature of high refractoriness under load, which decide high alumina brick is a n ideal material for various kinds of industrial furnace.
Application:
Fire clay brick is widely used in building lining of hot-blast stove, blast furnace, coke oven, rotary kilns of cement and so on.
Technical Index:
Item | Chamotte Brick for Carbon Furnace | ||||||||
N-1 | N-2a | N-2b | N-3a | N-3b | N-4 | N-5 | N-6 | ||
Al2O3 % | ≥42 | ≥40 | ≥40 | ≥40 | ≥40 | ≥38 | -- | -- | |
Refractoriness ℃ | ≥1750 | ≥1730 | ≥1730 | ≥1710 | ≥1710 | ≥1690 | ≥1670 | ≥1580 | |
Refractoriness Under Load,℃,[0.2MPa×0.6%] | ≥1400 | ≥1350 | -- | ≥1320 | -- | ≥1300 | -- | -- | |
Permanent Linear Change, % | 1400℃×2h | +0.1 -0.4 | +0.1 -0.5 | +0.2 -0.5 | -- | -- | -- | -- | -- |
1350℃×2h | -- | -- | -- | +0.2 -0.5 | +0.2 -0.5 | +0.2 -0.5 | +0.2 -0.5 | -- | |
Apparent Porosity % | ≤22 | ≤26 | ≤24 | ≤24 | ≤26 | ≤24 | ≤26 | ≤28 | |
Cold Crushing Strength, MPa | ≥30.0 | ≥20.0 | ≥25.0 | ≥20.0 | ≥15.0 | ≥20.0 | ≥15.0 | ≥15.0 |
Manufacturing Process Flow:
Rough Materials-Mixing-Batching -Shaped-Drying-Sintering-Inspect-Packing-Delivery
FAQ:
1. Do you provide samples?
Standard size sample is free, but the air freight is collect or you pay us the cost in advance.
2. What’s your MOQ?
Normally we don’t have particular requirements on the MOQ. But we will charge the mold cost when the quantity of per shape is small.
3. What’s your warranty?
We are very confident in our products. Any quality issues, we will deal with it immediately.