Add to Cart
Refractory Heat Insulation Brick High Temperature Resistance Fire Clay Brick for Cement Kiln
The content of Al2O3 is 30% ~48%,
Refractoriness temperature is 1580~1750,
Refractoriness under load temperature is 1320-1400℃,
Made by clay clinker, soft clay or semi soft Clay as binder
Feature:
Low coefficient of linear expansion
Low thermal conductivity
Good erosion resistance
Excellent thermal shock resistance
High Refractoriness under load
Technical Index:
Item | Chamotte Brick for Carbon Furnace | ||||||||
N-1 | N-2a | N-2b | N-3a | N-3b | N-4 | N-5 | N-6 | ||
Al2O3 % | ≥42 | ≥40 | ≥40 | ≥40 | ≥40 | ≥38 | -- | -- | |
Refractoriness ℃ | ≥1750 | ≥1730 | ≥1730 | ≥1710 | ≥1710 | ≥1690 | ≥1670 | ≥1580 | |
Refractoriness Under Load,℃,[0.2MPa×0.6%] | ≥1400 | ≥1350 | -- | ≥1320 | -- | ≥1300 | -- | -- | |
Permanent Linear Change, % | 1400℃×2h |
+0.1 |
+0.1 |
+0.2 |
-- | -- | -- | -- | -- |
1350℃×2h | -- | -- | -- |
+0.2 |
+0.2 |
+0.2 |
+0.2 |
-- | |
Apparent Porosity % | ≤22 | ≤26 | ≤24 | ≤24 | ≤26 | ≤24 | ≤26 | ≤28 | |
Cold Crushing Strength, MPa | ≥30.0 | ≥20.0 | ≥25.0 | ≥20.0 | ≥15.0 | ≥20.0 | ≥15.0 | ≥15.0 |
FAQ:
1. Do you provide samples?
Standard size sample is free, but the air freight is collect or you pay us the cost in advance.
2. What’s your MOQ?
Normally we don’t have particular requirements on the MOQ. But we will charge the mold cost when the quantity of per shape is small.
3. What’s your warranty?
We are very confident in our products. Any quality issues, we will deal with it immediately.
Fire Clay Bricks Size or Shapes:
The shape can be customized according to the brick drawings.
Brick Size (mm) | |
Straight Shape | Side Arch |
230*114*65 250*123*65 171*113*65 230*114*20 230*114*30 230*114*40 230*57*65 520*230*113 650*230*113 780*230*113 452*230*65 230*150*75 345*150*75 |
230*65/55*114 230*65/45*114 230*65/55*171 230*65/45*171 230*114*65/55 230*114*65/45 230*150/120*75 230*150/110*75 |